FIELD: post-formation drying of active material of pasted negative plates for lead-acid batteries.
SUBSTANCE: proposed process for drying formed plates of lead-acid batteries is characterized in infrared irradiation at wavelength of 2 - 6 μm and temperature of 60 - 80 °C with air blowing at speed of 1 - 2 m/s until moisture content of negative plate active material, whose paste is made of pre-inhibited lead powder, is brought to 0.3 - 0.5%. Inhibition is made by aqueous solution of glycerin at density of 0.01 - 1.02g/cm3. Paste is irradiated for 10 -12 minutes by infrared radiators equally distributed on both ends of plates, their spatial position being chosen from following expression: b/h = 1.6, where b is distance from radiators to plates; h is distribution pitch of radiators; rows of infrared radiators spaced 45 mm apart are disposed at distance of 143 mm. Oxidability of active material obtained in the process is between 3.5 and 4.5% which is steadily maintained for long time when in contact with atmospheric air; paste embedded in plates is free from microcracks and does not exfoliate from plate grid.
EFFECT: enhanced quality of active material.
2 cl, 2 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
BATTERY PLATE DRYING DEVICE | 2004 |
|
RU2278451C1 |
METHOD FOR MANUFACTURING LEAD-ACID ACCUMULATOR | 2000 |
|
RU2177191C2 |
METHOD FOR MANUFACTURING OF NEGATIVE ELECTRODE OF LEAD STORAGE BATTERY | 1996 |
|
RU2128868C1 |
IMPROVED CONSTRUCTION OF LEAD-ACID BATTERY | 2013 |
|
RU2638532C2 |
LEAD-BASED ALLOY AND CORRESPONDING METHODS AND PRODUCTS | 2017 |
|
RU2699245C1 |
0 |
|
SU337858A1 | |
METHOD FOR MANUFACTURING BATTERY OF LEAD-ACID SYSTEM WITH SURFACE ELECTRODES | 2015 |
|
RU2634591C2 |
IMPROVEMENTS IN DESIGN OF LEAD-ACID ACCUMULATOR | 2010 |
|
RU2568667C2 |
0 |
|
SU1784106A3 | |
PROCESS OF MANUFACTURE OF ACTIVE MASSES FOR ELECTRODES OF STORAGE CELLS | 1991 |
|
RU2012950C1 |
Authors
Dates
2006-03-20—Published
2004-11-26—Filed