FIELD: technological processes.
SUBSTANCE: invention can be used in the preparation of fluoride salts used in the production of aluminum by electrolysis. Treatment of the regeneration cryolite is carried out with aluminum sulfate or aluminum chloride at a temperature of 60–80 °C for 20–120 minutes while maintaining pH 2–4. After this, the product is dehydrated and dried. Invention makes it possible to obtain a mixture of cryolite and chiolite with a low sodium content without the use of hydrofluoric acid and corrosion-resistant equipment.
EFFECT: reduced sodium content in the regenerated fluoride salts allows to return more salts to production.
1 cl, 1 dwg, 3 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING ALUMINIUM FLUORIDE | 2011 |
|
RU2462418C1 |
METHOD OF OBTAINING HYDROGEN FLUORIDE | 2012 |
|
RU2505476C1 |
METHOD OF PROCESSING SPENT LINING OF ALUMINIUM ELECTROLYTIC CELL | 2015 |
|
RU2609478C1 |
METHOD FOR CRYOLITE PRODUCTION | 0 |
|
SU1801101A3 |
PROCEDURE FOR PROCESSING FLUORINE-CONTAINING MATERIALS USED IN ELECTROLYTIC PRODUCTION OF ALUMINIUM | 2009 |
|
RU2402621C1 |
METHOD OF PRODUCING ALKALI-FREE MINERALIZER FOR BURNING CLINKER FROM FLUORINE-CONTAINING WASTES OF ALUMINIUM PRODUCTION | 2023 |
|
RU2821274C1 |
PROCESS FOR PRODUCING CRYOLITE | 0 |
|
SU929561A1 |
METHOD FOR PROCESSING SPENT THERMAL INSULATION LINING OF ALUMINIUM ELECTROLYSER | 2016 |
|
RU2643675C1 |
METHOD OF PRODUCING SYNTHETIC FLUORITE AND CAUSTIC SODA SOLUTION | 2023 |
|
RU2816485C1 |
CRYOLITE PRODUCTION METHOD | 0 |
|
SU1047836A1 |
Authors
Dates
2018-09-19—Published
2017-09-21—Filed