FIELD: polymer materials.
SUBSTANCE: invention provides a method for manufacturing polyvinyl alcohol-based modified films with elevated fire resistance by means treatment with phosphorus-containing compounds. In particular, 5-15% aqueous solution of methyl phosphite borate is used and films are treated during 1-2 min and then dried at ambient temperature. Thus obtained polymers are characterized by good film-forming properties, exhibit self-extinction capability, and show water absorption at a level of 1.14%. Films can be used in various industry and national economy fields.
EFFECT: improved performance characteristics of films.
1 tbl, 3 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD FOR PREPARATION OF MODIFIED FILMS BASED ON POLYVINYL ALCOHOL | 2008 | 
 | RU2359976C1 | 
| METHOD OF MANUFACTURING MODIFIED CELLULOSE MATERIALS | 2003 | 
 | RU2254341C1 | 
| METHOD OF OBTAINING MODIFIED FILMS BASED ON POLYVINYL ALCOHOL | 2007 | 
 | RU2355707C1 | 
| COMPOSITION FOR OBTAINING FILMS BASED ON POLYVINYL ALCOHOL | 2008 | 
 | RU2362790C1 | 
| METHOD FOR PRODUCTION OF MODIFIED PAPER | 2007 | 
 | RU2355842C1 | 
| COMPOUND FOR PRODUCTION OF MODIFIED PAPER | 2008 | 
 | RU2355841C1 | 
| PHOSPHORUS-BORON-CONTAINING METHACRYLATE AS POLYVINYL ALCOHOL-BASE FILM MATERIAL COMBUSTION INHIBITOR | 2003 | 
 | RU2254327C1 | 
| METHOD OF MODIFYING SYNTHETIC FIBRE | 2007 | 
 | RU2330136C1 | 
| METHOD OF MODIFYING POLYESTER FIBRE | 2012 | 
 | RU2487205C1 | 
| METHOD FOR MODIFICATION OF POLYAMIDE FIBRES | 2008 | 
 | RU2378427C1 | 
Authors
Dates
2006-06-27—Published
2004-06-07—Filed