FIELD: textile, paper.
SUBSTANCE: invention relates to production technology of synthetic paper, precisely to production of modified paper with higher gas-proof and heat-protective properties, and can be applied in constructions, aircraft and automobile constructions, shipbuilding. The compound contains 5-7% aqueous solution of polyvinyl alcohol, 15-20% aqueous solution of methyl phosphate borate and 5-7% aqueous solution of chitosan at the following ratio, pts. wt. polyvinyl alcohol - 5-7; chitosan - 5-7; methyl phosphate borate - 15-20; water - 275-266.
EFFECT: increase of gas-proof and heat-protective properties, and resistance to thermal-oxidative degradation of modified paper.
2 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF MODIFIED PAPER | 2007 |
|
RU2355842C1 |
MODIFYING COMPOSITION FOR FILMS BASED ON POLYVINYL ALCOHOL | 2007 |
|
RU2355708C1 |
METHOD OF OBTAINING MODIFIED FILMS BASED ON POLYVINYL ALCOHOL | 2007 |
|
RU2355707C1 |
COMPOSITION FOR FIRE-RESISTANT TREATMENT OF POLYAMIDE FIBRES | 2008 |
|
RU2378428C1 |
METHOD FOR MODIFICATION OF POLYAMIDE FIBRES | 2008 |
|
RU2378427C1 |
METHOD OF MANUFACTURING MODIFIED CELLULOSE MATERIALS | 2003 |
|
RU2254341C1 |
METHOD OF MODIFYING POLYESTER FIBRE | 2012 |
|
RU2487205C1 |
COMPOSITION FOR OBTAINING FILMS BASED ON POLYVINYL ALCOHOL | 2008 |
|
RU2362790C1 |
COMPOSITION FOR FIREPROOF PROCESSING OF POLYAMIDE FIBRES | 2007 |
|
RU2344215C1 |
METHOD FOR PREPARATION OF MODIFIED FILMS BASED ON POLYVINYL ALCOHOL | 2008 |
|
RU2359976C1 |
Authors
Dates
2009-05-20—Published
2008-01-09—Filed