FIELD: textile, paper.
SUBSTANCE: invention relates to papermaking technology, precisely to production of modified paper with higher gas-proof and heat-protective properties, and can be applied in constructions, aircraft and automobile constructions, shipbuilding. The method includes treatment of paper with the mixture of 5-7% aqueous solution of polyvinyl alcohol with 5-7% aqueous solution of chitosan at their ratio 1:1 within 10-15 minutes, thereafter treatment with 15-20% aqueous solution of methyl phosphate borate and drying.
EFFECT: prepared modified paper has increased gas-proof and heat-protective properties, and resistance to thermal-oxidative degradation.
1 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
COMPOUND FOR PRODUCTION OF MODIFIED PAPER | 2008 |
|
RU2355841C1 |
METHOD OF OBTAINING MODIFIED FILMS BASED ON POLYVINYL ALCOHOL | 2007 |
|
RU2355707C1 |
MODIFYING COMPOSITION FOR FILMS BASED ON POLYVINYL ALCOHOL | 2007 |
|
RU2355708C1 |
METHOD OF MANUFACTURING MODIFIED CELLULOSE MATERIALS | 2003 |
|
RU2254341C1 |
METHOD FOR MODIFICATION OF POLYAMIDE FIBRES | 2008 |
|
RU2378427C1 |
COMPOSITION FOR FIRE-RESISTANT TREATMENT OF POLYAMIDE FIBRES | 2008 |
|
RU2378428C1 |
METHOD OF MODIFYING POLYESTER FIBRE | 2012 |
|
RU2487205C1 |
METHOD FOR PREPARATION OF MODIFIED FILMS BASED ON POLYVINYL ALCOHOL | 2008 |
|
RU2359976C1 |
METHOD FOR MODIFICATION OF POLYAMIDE FIBERS | 2007 |
|
RU2346095C1 |
METHOD OF MANUFACTURING POLYVINYL ALCOHOL-BASED MODIFIED FILMS | 2004 |
|
RU2278874C2 |
Authors
Dates
2009-05-20—Published
2007-12-27—Filed