FIELD: recovery of radioactive wastes.
SUBSTANCE: proposed method for matrix immobilization of industrial wastes includes preparation of source solution of industrial wastes and impregnation of ceramic matrix with this solution followed by roasting this matrix; source liquid radioactive wastes used for the purpose are first treated with promoter crystallization solution doped with oxide-forming admixtures whereupon radioactive wastes are introduced in ceramic matrix and roasted using microwave energy at temperature of 900 - 1 000 °C. Such procedure provides for recovering great amount of radioactive wastes included and chemically bonded in ceramic matrix which makes it possible to reduce leaching and to enhance matrix strength and life.
EFFECT: facilitated procedure, reduced cost, enhanced quality of radioactive waste immobilization and environmental friendliness.
1 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SYNTHESIZING MINERAL-LIKE MATRICES FOR ISOLATION OF RADIOACTIVE SUBSTANCES | 2016 |
|
RU2633817C1 |
METHOD FOR PRODUCTION OF MINERAL-LIKE MATRIX FOR IMMOBILIZATION OF HIGHLY ACTIVE WASTE | 2021 |
|
RU2790580C2 |
METHOD OF IMMOBILISATION OF ISOTOPES OF RADIOACTIVE WASTES OF TRANSURANIC ELEMENTS (VERSIONS) | 2007 |
|
RU2361299C1 |
METHOD OF LONG-LIVE RADIONUCLIDE IMMOBILISATION | 2007 |
|
RU2340968C1 |
METHOD OF IMMOBILISING STRONTIUM-CAESIUM FRACTION OF HIGHLY ACTIVE WASTES BY INCORPORATION INTO GEO-CERAMIC MATRICES | 2014 |
|
RU2561508C1 |
METHOD OF IMMOBILIZATION OF LIQUID HIGH-SALT RADIOACTIVE WASTE | 2017 |
|
RU2645737C1 |
IMMOBILISATION METHOD OF RADIONUCLIDES OF ALKALINE-EARTH AND RARE-EARTH ELEMENTS IN MINERAL MATRIX | 2010 |
|
RU2444800C1 |
METHOD TO IMMOBILISE RADIOACTIVE WASTES IN MINERAL-LIKE MATRIX | 2010 |
|
RU2439726C1 |
PROCESS OF PROCESSING OF HIGH-TOXIC INDUSTRIAL WASTE | 2001 |
|
RU2176417C1 |
METHOD FOR RECOVERING LIQUID RADIOACTIVE WASTE (ALTERNATIVES) | 2006 |
|
RU2321909C1 |
Authors
Dates
2006-08-10—Published
2005-06-02—Filed