FIELD: composition for corrosion protection of basic constructional materials (steel, concrete).
SUBSTANCE: claimed composition contains (mass %): polymeric film-forming substance 40-52; natural fine-grain iron alpha-oxide 11-27; organosilicon curing agent 1`2-17; thiocol 7-10; synthetic silica 3-5; strontium chromate 7-9. Solution of epoxy resin in xylene and acetone is used as polymeric film-forming substance. Natural fine-grain iron alpha-oxide contains (mass %): silica, aluminum oxide, magnesium oxide, and calcium oxide not more than 2.5; 1.8, 0.2, and 0.3, respectively and Fe2O3 85-95 %. As organosilicon curing agent organosilicon amine derivatives are used.
EFFECT: coating of increased fuel resistant and durability in high aggressive medium, containing, in particular, fuel with water impurity.
2 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR APPLYING ANTICORROSIVE COATING | 2005 |
|
RU2284342C1 |
COMPOSITION FOR ANTICORROSION COATING (VARIANTS) | 2005 |
|
RU2283330C1 |
COMPOSITION FOR CORROSION-DESISTANT COATING | 1999 |
|
RU2174136C2 |
COMPOSITION FOR APPLICATION OF ANTI-CORROSION COATING | 2013 |
|
RU2563794C2 |
COMPOSITION FOR APPLICATION OF ANTICORROSION COATING | 2012 |
|
RU2538878C2 |
COMPOSITION AND SYSTEM FOR ANTICORROSION COATING | 2007 |
|
RU2358998C2 |
COMPOSITION FOR A METAL COATING | 2004 |
|
RU2260610C1 |
COMPOSITION FOR ANTI-CORROSION COATING | 2014 |
|
RU2574512C1 |
ABRASION-RESISTANT PROTECTIVE POLYMERIC COMPOSITION | 2004 |
|
RU2261879C1 |
WEAR-RESISTANT PROTECTIVE POLYMER COMPOSITION | 2007 |
|
RU2374282C2 |
Authors
Dates
2006-09-10—Published
2005-04-28—Filed