FIELD: chemical technology.
SUBSTANCE: invention is designated for utilization of rubber crumbs prepared from used up tires. Rubber crumbs in mixture with heavy petroleum residues in the ratio = (10:90)-(40:60) are subjected for thermal oxidation with air at temperature 250-300°C or by thermal treatment at temperature 280-320°C followed by oxidation with air at temperature 230-270°C to yield the modified bitumen material. Prepared product shows adhesion to marble and granite 100%, reduced temperature dependence of index "penetration" and can be used as binding material in road building, insulating works and in another fields.
EFFECT: improved method for utilization.
2 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD AND DEVICE FOR SALVAGING OF USED UP TYRES AND WASTE OF MECHANICAL RUBBER GOODS | 1998 |
|
RU2153415C2 |
BINDER (POLYETHYLENE-TAR BINDER WITH RUBBER CRUMB - PERB-R) FOR ROAD COVERING | 2012 |
|
RU2519214C1 |
METHOD OF PROCESSING RUBBER-CONTAINING WASTES | 2009 |
|
RU2394852C1 |
METHOD FOR PRODUCTION OF MODIFIED BITUMINOUS BINDERS FOR ROAD SURFACES (VERSIONS) | 2016 |
|
RU2630529C1 |
BINDER (POLYETHYLENE-TAR BINDER PETB) FOR ROAD COVERING | 2012 |
|
RU2519207C1 |
RUBBER-BITUMEN ROAD BINDER FOR ASPHALT-CONCRETE MIXTURE | 2018 |
|
RU2707770C1 |
METHOD FOR BITUMEN PRODUCTION | 2009 |
|
RU2405807C1 |
RUBBER-POLYMER-BITUMEN BINDER AND METHOD FOR PRODUCTION THEREOF | 2020 |
|
RU2752619C1 |
METHOD OF PRODUCING BITUMEN-POLYMER MATERIALS | 2003 |
|
RU2265033C2 |
LOW-TEMPERATURE METHOD OF PRODUCING MODIFIED RUBBER CRUMBS | 2020 |
|
RU2730857C1 |
Authors
Dates
2006-11-10—Published
2004-12-24—Filed