FIELD: iodide refining of hafnium.
SUBSTANCE: interaction of iodine with black metal is carried out at temperature of 250-350°C. Sedimentation of refined hafnium is carried out at temperature of 1200-1600°C on heater (filament) made from molybdenum or zirconium wire in form of one or several loops connected to electrode end-pieces. Heater is formed in iodide refining apparatus in such way that lower part of each wire loop is suspended above insulator surface at clearance equal to 1/3-1/2 of final thickness of bar. Proposed method may be used for production of iodide hafnium bars more than 17 mm in diameter at height of heater loop more than 0.8 m.
EFFECT: enhanced purity by admixtures.
4 cl, 1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
APPARATUS FOR IODIDE REFINING OF ZIRCONIUM | 2003 |
|
RU2261287C2 |
METHOD FOR PRODUCING HAFNIUM BY IODIDE REFINING | 2022 |
|
RU2784718C1 |
INSTRUMENT FOR IODIDE REFINED HAFNIUM | 2007 |
|
RU2353687C1 |
METHOD FOR PRODUCTION OF HIGH-PURITY ZIRCONIUM OF HAFNIUM | 1993 |
|
RU2048558C1 |
METHOD OF PRODUCTION OF HIGH PURITY TITANIUM FOR SPUTTERED TARGETS | 2008 |
|
RU2370559C1 |
METHOD OF CONTROLLING TEMPERATURE MODE OF PROCESS OF IODIDE REFINING OF ZIRCONIUM | 1991 |
|
RU2016107C1 |
METHOD FOR IODIDE REFINEMENT OF ZIRCONIUM AND APPARATUS THEREFOR | 2012 |
|
RU2532208C2 |
PROCESS FOR PRODUCTION OF REFINED BILLETS FROM METAL OF TITANIUM GROUP AND ALLOYS ON ITS BASIS | 1996 |
|
RU2107585C1 |
PROCEDURE FOR CONTROL OVER PROCESS OF ZIRCONIUM IODIDE REFINING AND SYSTEM FOR ITS IMPLEMENTATION | 2010 |
|
RU2421530C1 |
METHOD OF OBTAINING SEMI-FINISHED PRODUCT FROM ALLOY ON BASIS OF NIOBIUM | 2018 |
|
RU2680321C1 |
Authors
Dates
2007-01-10—Published
2004-11-29—Filed