FIELD: mechanical engineering; production of foil from beryllium.
SUBSTANCE: proposed method consists in placing the beryllium blank into metal casing, sealing-up, rolling at temperature of 600-800°C and removal of casing. Prior to placing the blank into casing, it is placed into solution for passivation and is heated in air at temperature of 550-600°C during period sufficient for forming modified passive film up to 10 mcm in thickness; passivation solution contains the following components, g/l: potassium bichromate, 150-200; hydrofluoric acid, 9.5-9.8; sodium fluoride, 5-10; beryllium, 0.2-0.4; water, up to 1 l. Proposed method excludes fusion of beryllium blank with metal of casing in rolling and contamination of beryllium with alloying elements of metal of casing.
EFFECT: enhanced mechanical properties of foil; increased vacuum density at retained radiation transparence.
3 cl, 3 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING THIN VACUUM-TIGHT BERYLLIUM FOIL | 2019 |
|
RU2739457C1 |
METHOD OF PRODUCING VACUUM-TIGHT FOIL FROM BERYLLIUM | 2019 |
|
RU2731636C1 |
METHOD OF MAKING HIGH-PURITY VACUUM-SEALED FOIL FROM BERYLLIUM | 2012 |
|
RU2497611C1 |
METHOD FOR HEAT TREATMENT OF BERYLLIUM COMPONENTS | 1992 |
|
RU2005807C1 |
0 |
|
SU1779420A1 | |
THIN BERYLLIUM FOIL PRODUCTION METHOD | 1989 |
|
RU2036244C1 |
METHOD AND APPARATUS FOR PRODUCING BERYLLIUM OR BERYLLIUM-CONTAINING FOIL | 2000 |
|
RU2194087C2 |
METHOD FOR PREPARING COVER MADE OF BERYLLIUM | 1985 |
|
SU1840477A1 |
COPPER-BASE SOLDER | 2004 |
|
RU2279957C1 |
METHOD FOR MAKING ARTICLES OF METALLIC ALLOY SUBJECTED TO COLD WORKING (VARIANTS) | 2000 |
|
RU2245760C2 |
Authors
Dates
2007-05-20—Published
2005-12-27—Filed