FIELD: electrical engineering; recovering storage batteries.
SUBSTANCE: proposed method for recovering lead storage batteries includes washing of active material covering positive plates and grid with distilled water, its drying, crushing, heat treatment at temperature of 450 - 500 °C to yellow color, whereupon paste is prepared by mixing powder with distilled water followed by addition of sulfuric acid solution of 1.40 g/cm3 specific gravity while intensively stirring it, its rubbing into plate in single operation, and compacting by rolling it first between rubber rolls, drying out at 120 °C for 20 - 25 s or weathering for 4 - 6 min, repeated rolling between rolls wrapped in gauze; ready plates are exposed to temperature of 45 - 50 °C and air humidity of minimum 95 % for 16 - 18 h, then held at same temperature and humidity reduced to 76 % for another 20 h, and dried out at temperature of 68 - 70 °C and air humidity of maximum 20 % for 12 - 14 h; negative plates with swollen active material are recovered without removal of active material from grids by compressing them with canvas spacers; prior to compressing negative plates are held in sulfuric acid of 1.83 g/cm3 specific gravity at temperature of 50 - 60 °C for 25 - 26 h, washed in distilled water, air-dried for 25- 26 h, washed with distilled water, air-dried for 1 - 2 h, and charged upon assembling the battery.
EFFECT: extended service life of recovered batteries, reduced their self-discharge and material input, enhanced use factor of source material.
1 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR RESTORING LEAD ACCUMULATORS | 2004 |
|
RU2294582C2 |
METHOD FOR RECONDITIONING STORAGE BATTERIES | 1999 |
|
RU2158047C1 |
STORAGE BATTERY RESTORATION METHOD AND DEVICE FOR ITS IMPLEMENTATION | 2009 |
|
RU2437190C2 |
METHOD OF RECONDITIONING OF LEAD ACID STORAGE BATTERIES | 1994 |
|
RU2076403C1 |
PRODUCTION TECHNIQUE OF SURFACE-TYPE NEGATIVE ELECTRODE FOR LEAD-ACID BATTERY | 2015 |
|
RU2648246C2 |
PROCESS OF MANUFACTURE OF ACTIVE MASSES FOR ELECTRODES OF STORAGE CELLS | 1991 |
|
RU2012950C1 |
ADDITIVE FOR SULFURIC-ACID ELECTROLYTE AND METHOD OF USE OF SUCH ADDITIVE | 2004 |
|
RU2267191C1 |
METHOD FOR REGENERATION OF WASTE STORAGE BATTERIES | 1996 |
|
RU2088002C1 |
PROCESS OF MANUFACTURE OF NEGATIVE ELECTRODE OF LEAD-ACID CELL | 1989 |
|
RU1715157C |
METHOD FOR EVALUATING FS EXPANDER IN ACTIVE MATERIAL OF LEAD-ACID BATTERY NEGATIVE PLATE | 2004 |
|
RU2279160C1 |
Authors
Dates
2007-06-27—Published
2005-11-21—Filed