FIELD: production of inorganic ceramic pigments.
SUBSTANCE: charge contains cobalt oxide (III), aluminum oxide, powder-like aluminum and additionally zinc oxide at the following ratio of components, mass-%: cobalt oxide CO2O3, 43-46; aluminum oxide Al2O3, 44-48; aluminum Al, 7-10; zinc oxide ZnO, 2-5. Charge of such composition is thoroughly mixed and is poured into screen made from stainless steel. Then, charge is heated to temperature of 500C for obtaining layer-by-layer burning effected from incendiary tablet Ni+Al (50 at.% Al) initiated by electric igniter. Thermosynthesis of pigment is carried out under conditions of layer-by-layer burning and natural filtration ensuring easy removal of gases formed in the course of synthesis.
EFFECT: enhanced efficiency; improved pigment color characteristics.
2 cl, 1 dwg, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING CERAMIC PIGMENTS OF SPINEL TYPE | 2015 |
|
RU2580542C1 |
METHOD OF PRODUCING CERAMIC PIGMENTS BASED ON ALUMINIUM-MAGNESIUM SPINEL | 2015 |
|
RU2580343C1 |
FEEDSTOCK FOR PRODUCING CERAMIC DARK-BLUE PIGMENT | 1996 |
|
RU2097346C1 |
METHOD OF PREPARING CERAMIC PIGMENT | 1997 |
|
RU2120918C1 |
METHOD OF PREPARING CERAMIC PIGMENT | 1997 |
|
RU2121463C1 |
CHARGE FOR CERAMIC PIGMENT | 1992 |
|
RU2029745C1 |
METHOD OF PREPARING SUPPORTED CATALYSTS | 2005 |
|
RU2284219C1 |
MIXTURE FOR PRODUCTION OF CERAMIC PIGMENT COLORED MARINE BLUE | 1992 |
|
RU2057729C1 |
METHOD OF PREPARING SUPPORTED CATALYSTS | 2003 |
|
RU2234979C1 |
CHARGE FOR PRODUCTION OF CERAMIC PIGMENT OF BLUE-GREEN COLOUR | 2008 |
|
RU2358922C1 |
Authors
Dates
2007-08-27—Published
2005-02-28—Filed