FIELD: technology of silicates; materials technology.
SUBSTANCE: proposed method includes preliminary dry molding of concentrate by pouring dry concentrate into ingot mold, mullitization at temperature of 1100-1300°C and sintering at temperature of 1400-1500°C. Prior to sintering, semi-finished product is subjected to mechanical treatment for obtaining required geometric shape.
EFFECT: possibility of obtaining articles of intricate shape at simplified technology.
2 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PREPARING MULLITE FROM KAOLIN | 2006 |
|
RU2312940C1 |
METHOD OF OBTAINING MULLITE FROM TOPAZ CONCENTRATE | 2007 |
|
RU2335481C1 |
BLEND FOR MANUFACTURING CHAMOTTE REFRACTORY MATERIALS | 2001 |
|
RU2213713C2 |
METHOD OF PREPARING MULLITE FROM TOPAZ CONCENTRATE | 2004 |
|
RU2287502C2 |
BLEND FOR MANUFACTURING CHAMOTTE REFRACTORY MATERIALS | 2001 |
|
RU2198150C2 |
METHOD OF MANUFACTURING CORUNDUM REFRACTORY PRODUCTS | 2005 |
|
RU2271345C1 |
CRUDE MIXTURE AND METHOD OF PRODUCING HIGH-STRENGTH REFRACTORY CERAMIC BASED ON SAID MIXTURE | 2009 |
|
RU2422405C1 |
CHARGE FOR MAKING SAGGER FURNITURE | 0 |
|
SU893957A1 |
METHOD OF PRODUCTION OF MULLITE OUT OF THE QUARTZ-TOPAZ RAW MATERIALS | 2004 |
|
RU2272854C1 |
METHOD FOR MANUFACTURING CORUNDOMULLITE REFRACTORY PRODUCTS | 2020 |
|
RU2756300C1 |
Authors
Dates
2008-01-27—Published
2006-04-14—Filed