FIELD: manufacture of electroluminescent devices.
SUBSTANCE: proposed charge contains the following components, mass-%: copper monochloride CuCl, 0.05-0.15; manganese fluoride MnF2·3H2O, 0.2-0.45 or manganous nitrate Mn(NO3)2·6H2O, 0.196-0.43; ammonium halogenide, 0.5-1.5; zinc chloride ZnCl2·2H2O, 0.25-1; or zinc bromide ZnBr2, 0.28-1.2; oxalic acid, H2C2O4·2H2O or hydrazine sulfate (NH2OH)2·H2SO4, or hydroxylamine hydrosulfate NH2OH·HCl, 1-3; sulfur, 2-4; the remainder being zinc sulfide ZnS. Charge may contain ammonium chloride NH4Cl, ammonium bromide NH4Br or ammonium iodide NH4J used as ammonium halogenide. Charge components are thoroughly mixed, sieved and calcined in reducing atmosphere at temperature of 850-1050°C. Calcined luminophor is cooled, sorted out and subjected to chemical treatment, dried and sieved afterwards. Proposed charge increases luminosity by 2 times.
EFFECT: intensified luminosity; increased service life of articles; possibility of changing the color at constant level of brightness.
2 cl, 2 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
0 |
|
SU510497A1 | |
METHOD OF PRODUCING POWDERED ZINC SULPHIDE ELECTROLUMINESCENT MATERIAL | 2009 |
|
RU2425085C1 |
METHOD OF MAKING ZINC SULPHIDE ELECTROLUMINESCENT MATERIAL | 2007 |
|
RU2390534C2 |
0 |
|
SU276294A1 | |
METHOD OF PRODUCING POWDERED ZINC SULPHIDE ELECTROLUMINESCENT MATERIAL | 2010 |
|
RU2429271C1 |
0 |
|
SU186057A1 | |
0 |
|
SU472967A1 | |
0 |
|
SU233817A1 | |
METHOD FOR TREATING ELECTROPHOSPHOR BASED ON ZINC SULFIDE | 0 |
|
SU1114692A1 |
CHARGE TO PRODUCE THE LONG-LIVED AFTERGLOW LUMINOPHOR ON THE BASE OF ZINC SULFIDE | 2001 |
|
RU2217466C2 |
Authors
Dates
2008-01-27—Published
2006-03-20—Filed