FIELD: ferrous metallurgy, in particular, process for blast-furnace melting of zinc-containing burden.
SUBSTANCE: method involves removing zinc from furnace working space by forming buffer layer having predetermined height through charging of coke and crushed slag and periodically lowering burden charge level; forming buffer layer from individual coke layer and crushed slag layer of fractions, respectively, (25-150):(40-150) mm, with weight ratio of components, respectively, (20-60):(150-300) kg/m3 of blast furnace; elevating temperature of blast furnace gas to 420-750 C, said process being carried out in 25-35 days; feeding blast-furnace gas cleaner sledges into separate sledge collector and providing natural settling of sledge during at least 3 days; pumping pulp of settled sledge; dehydrating and unloading dried sledge for zinc production.
EFFECT: reduced periodicity in repairing of blast furnace, reduced consumption of coke, and increased efficiency of blast furnace.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MELTING ZINC CONTAINING CHARGES IN BLAST FURNACE | 2004 |
|
RU2280080C2 |
METHOD OF BLAST-FURNACE SMELTING OF ALKALI-ZINC-CONTAINING CHARGES | 2003 |
|
RU2237721C1 |
METHOD FOR BLAST SMELTING OF ZINC-CONTAINING BURDEN | 2000 |
|
RU2186117C2 |
METHOD OF BLAST FURNACE HEAT | 1996 |
|
RU2074893C1 |
METHOD OF BLAST-FURNACE MELTING OF ZINC CONTAINING CHARGE | 2019 |
|
RU2709179C1 |
METHOD OF A BLAST FURNACE SMELTING OF ZINC-CONTAINING BLENDS | 2004 |
|
RU2252970C1 |
BLAST-FURNACE FUSION OF ALKALINE MATERIALS | 2012 |
|
RU2533239C2 |
PROCESS FOR BLAST FURNACE OPERATION | 0 |
|
SU1640173A1 |
PROCESS FOR BLAST FURNACE SMELTING OF ZINC-CONTAINING CHARGE | 1992 |
|
RU2025491C1 |
BRIQUETTE FOR MELTING OF MANGANESE-CONTAINING CAST IRON | 2005 |
|
RU2308493C2 |
Authors
Dates
2008-04-10—Published
2006-03-15—Filed