Abstract RU 2336235 C1

FIELD: chemistry.

SUBSTANCE: glass contains the following components in wt %: SiO2 - 55-70; Al2O3 - 0.1-5; B2O3 - 0.1-8; Na2O - 10-20; CaO - 0.1-7; SrO - 0.1-5.5; P2O5 - 0.2-6; ZnO - 0.1-11; BaO - 0.1-6.2; K2O - 0.1-5.0; CeO2 - 0.3-2; F - 0.2-7; TiO2 - 0.1-4. Glass has the following properties: value of temperature coefficient of linear expansion equals 79-86-10-7 1/°C; amount of released crystal phase is not more than 4 wt %.

EFFECT: increase of thermosensitivity effect.

2 tbl

Similar patents RU2336235C1

Title Year Author Number
GLASS 2006
  • Shchepochkina Julija Alekseevna
RU2315010C1
GLASS 2006
  • Shchepochkina Julija Alekseevna
RU2316490C1
THERMOSENSITIVE GLASS 1993
  • Varshal B.G.
  • Kisljak Z.N.
  • Kolchenova T.N.
  • Stepin V.I.
  • Starovojtov V.V.
  • Sharin V.A.
  • Guseva L.V.
RU2098365C1
GLAZE 2012
  • Afanas'Ev Sergej Vasil'Evich
  • Makhlaj Sergej Vladimirovich
RU2498951C1
RADIOPAQUE GLASS FOR FILLER OF COMPOSITE DENTAL MATERIALS 2023
  • Savinkov Vitalij Ivanovich
  • Zinina Enzhegel Mansurovna
  • Klimenko Nataliya Nikolaevna
  • Sigaev Vladimir Nikolaevich
  • Posokhova Vera Fedorovna
  • Chuev Vladimir Petrovich
  • Buzov Andrej Anatolevich
  • Kazakova Valentina Sergeevna
RU2816453C1
GLASS FOR MAKING BEADS 2006
  • Shchepochkina Julija Alekseevna
RU2302382C1
GLASS 2006
  • Shchepochkina Julija Alekseevna
RU2327656C1
CRYSTAL GLASS 2006
  • Shchepochkina Julija Alekseevna
RU2331595C1
GLASS 2006
  • Shchepochkina Julija Alekseevna
RU2335466C1
GLASS 2006
  • Shchepochkina Julija Alekseevna
RU2325343C1

RU 2 336 235 C1

Authors

Ignatov Sergej Vladimirovich

Pavlushkina Tat'Jana Konstantinovna

Morozova Irina Vladimirovna

Dates

2008-10-20Published

2007-01-26Filed