FIELD: process flows; metallurgical engineering.
SUBSTANCE: method includes roller machining, heating for weld deposition at rate 50-100°C/hr to temperature from 250°C to 300°C, arc-jet weld deposition at electric current density 40-45A/mm2 with weld deposition rate from 25 m/hr to 30 m/hr and tempering for 1.5-2 hours at temperature 300-400°C.
EFFECT: improved resistance and performance of roller.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HARDENING OF STEEL ROLL OF SECTION ROLLING MILL | 2002 |
|
RU2228958C2 |
METHOD OF CAST IRON FORMING ROLL WOBBLERS REPAIR | 2006 |
|
RU2335387C2 |
METHOD FOR RESTORING CAST IRON ROLLING ROLLS WITH DAMAGED JOURNALS | 2004 |
|
RU2281846C1 |
METHOD FOR RESTORING ROLLING ROLLS | 1998 |
|
RU2139156C1 |
METHOD OF BUILDING UP ROLLS | 2002 |
|
RU2218220C1 |
PROCESS FOR RESTORING ROLLING ROLLS | 2003 |
|
RU2237563C1 |
METHOD FOR RESTORING ROLLING ROLLS | 2003 |
|
RU2245771C2 |
CAST IRON ROLL JOURNALS RESTORING METHOD | 2005 |
|
RU2283709C2 |
PROCEDURE FOR SURFACE STRENGTHENING OF FORMING ROLLS | 2009 |
|
RU2398892C1 |
METHOD OF RESTORING BACKUP ROLLS OF ROLLING MILL STANDS | 0 |
|
SU1804353A3 |
Authors
Dates
2008-11-27—Published
2006-10-31—Filed