FIELD: chemistry.
SUBSTANCE: proposed mixture for making an abrasive tool contains Rosoil-800 as a plasticiser with the following ratio of components: synthetic solid high-molecular rubber 80÷90; synthetic low-molecular rubber 10÷20; sulphur 20÷35; captax 2.5÷3.0; filler 20÷100; plasticiser Rosoil-800 3÷8; abrasive substance 700÷1000.
EFFECT: higher porosity of the abrasive tool with retention of mechanical strength, increased cutting ability of the tool and reduced thermal damage to the processed metal.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
PASTE FOR MANUFACTURING ABRASIVE TOOLS | 2004 |
|
RU2269408C2 |
MASS FOR PRODUCING ABRASIVE TOOL | 2009 |
|
RU2413603C1 |
MASS FOR MAKING ABRASIVE TOOL | 2001 |
|
RU2200082C2 |
COMPOSITION FOR MANUFACTURING ABRASIVE TOOLS | 1990 |
|
RU2082597C1 |
COMPOSITION FOR MAKING POLISHING ABRASIVE ELASTIC WHEELS | 2005 |
|
RU2311280C2 |
MASS FOR PRODUCTION OF ABRASIVE WHEEL | 2009 |
|
RU2416507C1 |
STOCK MASS FOR MANUFACTURING ABRASIVE POLISHING TOOLS | 1994 |
|
RU2100385C1 |
VULCANISATION METHOD OF WORKPIECES OF RUBBER WHEELS | 2008 |
|
RU2376129C1 |
COMPOUND FOR POLISHING DENTAL HEADS USED TO PREPARE TEETH RESTORATIONS OF POLYMER COMPOSIT MATERIALS, GLASS IONOMER AND AMALGAMS | 2007 |
|
RU2372181C2 |
COMPOSITION MATERIAL FOR TRAUMATIC MISSILES OF FIREARMS | 2009 |
|
RU2404405C1 |
Authors
Dates
2009-02-10—Published
2007-05-07—Filed