FIELD: textile; paper.
SUBSTANCE: described is product, which has Brookfield viscosity within from approximately 700 to approximately 2500 cps, measured in accordance with method CRA B-54 with 0.5% of hard phase using spindle No 21 at 20 rot/min and temperature 97°C and method of obtaining starch products. Also described is application of cationic transversally bound wax-like starch products, which have Brookfield viscosity within from approximately 700 to approximately 2500 cps, in production of paper products, characterised by productivity 1.9 rolls per hour and inner binding strength 19.5 kPa/cm2.
EFFECT: described is cationic transversally bound wax-like starch product.
32 cl, 14 ex