FIELD: metallurgy.
SUBSTANCE: invention relates to extraction method of metallic elements, particularly, metallic chromium from slag, which contains oxides, particularly chrome oxide, in arc furnace. Additionally slag is not reduced at separated stage after melting, but there are implemented following stages: after charge introduction into arc furnace it is melted, forming molten metal and slag. Melt is discharged, keeping unreduced slag in furnace. Then it is fed following scrap portion, including reducers for slug. At melting of this charge slag is reduced. Then slag and melt are merged. Method can be used also in aggregates of ladle or convertermetallurgy.
EFFECT: reduction of melt handling total time for 15 minutes, reduction of ferrosilicon consumption and slag-forming consumption, life time increasing of furnace hearthstone and life time ladle plugs, improving of arc furnace energy balance.
7 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD AND PLANT FOR RECEIVING ALLOYED METAL MELT | 2004 |
|
RU2349647C2 |
COMPOSITE BLEND FOR SMELTING ALLOYED STEELS | 2001 |
|
RU2186856C1 |
METHOD OF PRODUCING HIGH TITANIUM FERROALLOY OUT OF ILMENITE | 2005 |
|
RU2329322C2 |
METHOD OF REPROCESSING ACCUMULATOR LEAD SCRAP | 1997 |
|
RU2119540C1 |
STEEL PRODUCTION METHOD AND LINE | 1994 |
|
RU2092572C1 |
METHOD FOR PRODUCING FERROMOLYBDENUM | 1994 |
|
RU2110596C1 |
METHOD FOR MAKING STEEL IN ELECTRIC-ARC FURNACE | 1995 |
|
RU2092574C1 |
METHOD TO MELT LOW-CARBON MANGANIFEROUS ALLOYS | 2010 |
|
RU2455379C1 |
METHOD OF PREPARING LOW-CARBON METALS AND ALLOYS | 2000 |
|
RU2164543C1 |
METHOD OF MANUFACTURING NICKEL ANODES | 1997 |
|
RU2120488C1 |
Authors
Dates
2009-04-20—Published
2004-04-23—Filed