FIELD: construction.
SUBSTANCE: glass and gasifier are ground, mixed, filled in molds and foamed. Glass fiber is additionally introduced in initial mixture at the following ratio of components, wt %: crushed glass - 49.0-60.0; glass fiber - 38.0-46.0; gasifier - 2.0-5.0, softening temperature of which exceeds glass softening temperature by 50-100°C.
EFFECT: improved strength of foam glass.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING FOAMED GLASS (VERSIONS) | 2010 |
|
RU2452701C1 |
METHOD OF PRODUCTION OF FOAM GLASS | 2013 |
|
RU2522606C1 |
FOAMGLASS | 2006 |
|
RU2336237C1 |
METHOD FOR MANUFACTURING OF GLASED GLASS FOAM | 2010 |
|
RU2431619C1 |
METHOD OF PRODUCING OF COLOURED FOAMED GLASS | 2013 |
|
RU2513823C1 |
RAW MIXTURE FOR MAKING FOAMED GLASS | 2009 |
|
RU2394000C1 |
METHOD OF FOAMED GLASS PRODUCTION | 2011 |
|
RU2502686C2 |
RAW MIXTURE USED FOR MANUFACTURING FOAM GLASS | 2008 |
|
RU2369571C1 |
MIXTURE FOR MANUFACTURING OF FACING TILES | 2010 |
|
RU2417193C1 |
MIXTURE FOR MAKING FOAMED GLASS | 2014 |
|
RU2563847C1 |
Authors
Dates
2009-07-20—Published
2007-11-26—Filed