FIELD: chemistry.
SUBSTANCE: ground silicate glass is mixed with a carbonate-containing gas-forming agent. The gas-forming agent is saturated with 3-5% aqueous cobalt nitrate or nickel nitrate or copper nitrate or manganese nitrate solution, followed by drying to constant mass. The mixture is laid down, dried, annealed and then cooled.
EFFECT: simple method of producing coloured foamed glass.
Title | Year | Author | Number |
---|---|---|---|
CHARGE FOR PRODUCING SILICATE MATERIAL | 2010 |
|
RU2449957C1 |
METHOD OF PRODUCING GLASS-CERAMITE | 2010 |
|
RU2413685C1 |
METHOD OF PRODUCING FOAMED GLASS (VERSIONS) | 2010 |
|
RU2452701C1 |
METHOD OF PRODUCING GLASS-CERAMITE | 2010 |
|
RU2417169C1 |
MATERIAL FOR EXTERIOR FINISH OF WALL PANELS | 2008 |
|
RU2375325C1 |
RAW MIX FOR PRODUCTION FOAM GLASS | 2007 |
|
RU2358927C1 |
METHOD OF GLASS PRODUCTION | 2009 |
|
RU2392239C1 |
METHOD FOR MANUFACTURE OF FOAM GLASS | 2007 |
|
RU2361828C1 |
RAW MIXTURE USED FOR MANUFACTURING FOAM GLASS | 2008 |
|
RU2369571C1 |
METHOD OF MANUFACTURING PRODUCTS FROM MULTI-LAYER HOLLOW GLASS | 2007 |
|
RU2352535C2 |
Authors
Dates
2014-04-20—Published
2013-02-19—Filed