FIELD: metallurgy.
SUBSTANCE: beforehand hardened alloy subject to cold deformation by means of multiple rolling with providing of total veritable degree of deformation e≥0.6 and annealing at temperature 250-550°C. Rolling is implemented with application to crumple zone of pulse current, parametres of which are variated in following intervals: current density 60-300 A/mm2, pulse-repetition frequency 400-1200 Hz and pulse duration 40-200 microsecond. Each following single clamping at multiple rolling is implemented with change of direction. Rolling rate amounts 20-250 mm/s. Parametres of pulse current is variated at each stage of deformation, herewith it is used unidirectional pulse current.
EFFECT: creation in alloys of regulated parametres of nanocrystalline structure with increased complex of mechanical and functional properties, reduction of laboriousness of technical process for receiving of semi-finished products.
5 cl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PROCESSING METHOD OF ULTRA-FINE-GRAINED ALLOYS WITH EFFECT OF SHAPE MEMORY | 2007 |
|
RU2367713C2 |
PROCESSING OF LONG ALUMINIUM ARTICLES | 2013 |
|
RU2537675C2 |
METHOD OF FORMING SEMIS FROM TITANIUM ALLOY BT6 | 2011 |
|
RU2479366C1 |
METHOD OF DEFORMATION TREATMENT OF LONG-DIMENSIONAL SEMI-FINISHED PRODUCTS OF THIN SECTION FROM TINI ALLOYS WITH SHAPE MEMORY EFFECT | 2018 |
|
RU2678855C1 |
METHOD OF PRODUCTION OF ULTRA-FINE-GRAINED TITANIUM-NICKEL ALLOYS OF MEMORIZED-SHAPE EFFECT | 2004 |
|
RU2266973C1 |
NANOSTRUCTURED TITANIUM-NICKEL ALLOY WITH SHAPE MEMORY EFFECT AND METHOD OF MAKING BAR THEREOF | 2012 |
|
RU2503733C1 |
METHOD OF OBTAINING LONG RIBS OF ULTRA-FINE-GRAIN TITANIUM-NICKEL ALLOYS WITH SHAPE MEMORY EFFECT | 2017 |
|
RU2685622C1 |
METHOD FOR PRODUCING BLANK OF Ti49,3Ni50,7 NANOSTRUCTURED ALLOY WITH SHAPE MEMORY EFFECT | 2016 |
|
RU2641207C1 |
NANO-STRUCTURAL TECHNICALLY PURE TITANIUM FOR BIO-MEDICINE AND METHOD OF PRODUCING WIRE OUT OF IT | 2008 |
|
RU2383654C1 |
METHOD FOR PRODUCING BLANKS FROM COMMERCIALLY PURE TITANIUM WITH GRAIN SIZE LESS THAN 0,4 MICRON | 2015 |
|
RU2622536C2 |
Authors
Dates
2009-09-20—Published
2007-09-19—Filed