FIELD: metallurgy.
SUBSTANCE: carburiser contains, wt %: silicon carbide 5-20, heat-treated coke is the rest. High and stable recovery rate of carbon by liquid metal is achieved owing to heat evolution from interaction of silicon carbide and high free surface energy of dispersed components of proposed carburiser. Carburiser corresponds to carbon-bearing materials, manufactured at high temperatures.
EFFECT: extra low content of nitrogen.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR METAL CARBONISATION | 2006 |
|
RU2339484C2 |
METHOD OF IRON SMELTING IN ELECTRIC ARC FURNACES | 2023 |
|
RU2823715C1 |
CARBONIZER (VERSIONS) | 2000 |
|
RU2175984C1 |
PROCEDURE FOR MELTING IRON-CARBON ALLOYS IN INDUCTION FURNACES | 2007 |
|
RU2395589C2 |
CARBONIZER (VERSIONS) | 2000 |
|
RU2191209C2 |
METHOD FOR OBTAINING NANOSTRUCTURED RECARBURISING AGENT FOR OUT-OF-FURNACE TREATMENT OF HIGH-STRENGTH CAST-IRON WITH BALL-SHAPED AND COMPACTED GRAPHITE | 2011 |
|
RU2495134C2 |
BRIQUETTE FOR IRON-CARBON ALLOY PRODUCTION (VARIANTS) | 2004 |
|
RU2282669C1 |
COMPLEX STEEL OXIDAZER BASED ON LUMPY SILICON CARBIDE | 2015 |
|
RU2631570C2 |
METHOD OF STEEL PRODUCTION IN ELECTRIC ARC FURNACE | 2015 |
|
RU2610975C2 |
PRODUCTION METHOD OF HIGH-STRENGTH CAST-IRONS WITH BALL-SHAPED OR COMPACTED GRAPHITE BASED ON NANOSTRUCTURED RECARBURISING AGENT | 2011 |
|
RU2495133C2 |
Authors
Dates
2010-01-27—Published
2006-11-07—Filed