FIELD: chemistry.
SUBSTANCE: in the method of treating quartz equipment for semiconductor production, involving treatment of quartz equipment after liquid operations of semiconductor production in a cleaning solution, the quartz equipment is treated with a cleaning solution which consists of hydrofluoric acid, ammonium fluoride, sulphomaleic anhydride and deionised water, with the following weight ratio of components 0.5:0.5:1:1 respectively. The quartz equipment is treated in two stages, the first at 30°C for 20-30 minutes, and the second in a fresh solution with the same weight ratio of components at room temperature for 10-20 minutes, after which the quartz equipment is treated with deionised water at room temperature for 30-60 minutes.
EFFECT: complete removal of different types of contaminations from the surface of quartz equipment, simple implementation of the method, reduced toxicity of the process.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF TREATING QUARTZ EQUIPMENT FOR SEMICONDUCTOR PRODUCTION | 2009 |
|
RU2386189C1 |
METHOD OF TREATING SILICON EQUIPMENT | 2008 |
|
RU2383965C1 |
METHOD OF QUARTZ PIPE CLEANING | 2013 |
|
RU2534446C2 |
METHOD OF QUARTZ GEAR PROCESSING | 2008 |
|
RU2366032C1 |
METHOD FOR CREATING ANTI-DIFFUSION BARRIER ON SURFACE OF PLATES MADE OF THERMOELECTRIC MATERIALS BASED ON BISMUTH AND ANTIMONY CHALCOGENIDES | 2021 |
|
RU2758989C1 |
METHOD OF PROCESSING SUBSTRATES IN LIQUID ETCHING AGENT | 2009 |
|
RU2419175C2 |
SELECTIVE BARIUM TITANATE ETCHANT | 2017 |
|
RU2674118C1 |
METHOD OF PRODUCING HIGH-PURITY BARIUM FLUORIDE | 2009 |
|
RU2424187C1 |
METHOD OF PRODUCING HIGH-PURITY CALCIUM FLUORIDE | 2009 |
|
RU2424188C1 |
METHOD OF PRODUCING HIGH-PURITY STRONTIUM FLUORIDE | 2009 |
|
RU2424189C1 |
Authors
Dates
2010-04-10—Published
2009-04-27—Filed