FIELD: chemistry.
SUBSTANCE: invention relates to production of polyamide resins in powder form. Spheroidal particles of polyamide or copolyesteramide with average diametre between 460 and 100 mcm are obtained through polymerisation in a solvent. The reaction medium is mixed with mineral filler - silica with average particle diametre between 1 and 30 µm. Polyamide or copolyester amide is obtained in powder form. The obtained powder is used to make coatings, ink compositions, paint compositions, cosmetic compositions, pharmaceutical compositions and alloys with metal powder or metal oxide powder. The polyamide or copolyester amide powder is used to make articles through oligomerisation by melting using a laser beam (laser sintering), infrared or UV radiation.
EFFECT: invention enables to obtain polyamide powder in form of particles with grain-size composition with average diametre between 60 and 100 mcm.
18 cl, 15 ex, 1 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
COSMETIC COMPOSITION CONTAINING FINELY DISPERSED AND POROUS POWDER | 2005 |
|
RU2313328C2 |
SEMIAROMATIC COPOLYAMIDE AND METHOD OF ITS OBTAINING | 2009 |
|
RU2511733C2 |
METHOD FOR SURFACE CROSS-LINKING OF POLYMER PARTICLES | 2014 |
|
RU2671508C2 |
SEMIAROMATIC POLYAMIDE WITH REGULATED CHAIN LENGTH | 2009 |
|
RU2510947C2 |
0 |
|
SU318228A1 | |
COMPOSITION CONTAINING COPOLYAMIDE AND CROSS-LINKED POLYOLEFIN | 2010 |
|
RU2496811C1 |
METHOD OF OBTAINING SPHERICAL PARTICLES ON POLYAMIDE BASE | 2004 |
|
RU2326134C2 |
0 |
|
SU321993A1 | |
METHOD OF OBTAINING THERMOPLASTIC POLYMER BASED PARTICLES AND POWDER OBTAINED USING SAID METHOD | 2007 |
|
RU2423399C2 |
METHOD OF PRODUCING PARTICLES BASED ON THERMOPLASTIC POLYMER AND POWDER, PRODUCED USING THIS METHOD | 2005 |
|
RU2358996C2 |
Authors
Dates
2010-07-27—Published
2005-11-10—Filed