FIELD: metallurgy.
SUBSTANCE: steel is heated to 1150-1250°C, cooled to 950-1100°C, and 30% plastic deformation at the above temperatures with further exposure in the air during 60±5 seconds and cooling in water is performed.
EFFECT: increasing yield point of austenitic steel at maintaining high level of ductility and impact strength characteristics.
1 ex, 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF PRODUCTION OF PLATE IRON OUT OF AUSTENITE NON MAGNETIC STEEL | 2008 | 
 | RU2366728C1 | 
| METHOD FOR OBTAINING HARDENED CYLINDRICAL BLANKS FROM AUSTENITIC STAINLESS STEEL | 2022 | 
 | RU2787279C1 | 
| METHOD FOR PRODUCING HARDENED WORKPIECES FROM NON-MAGNETIC CORROSION-RESISTANT AUSTENITIC STEEL | 2022 | 
 | RU2782370C1 | 
| HEAT TREATMENT METHOD OF CORROSION-RESISTANT MARTENSITE-AGING STEELS | 2013 | 
 | RU2535889C1 | 
| HIGH-STRENGTH NONMAGNETIC STEEL | 2010 | 
 | RU2447186C2 | 
| METHOD FOR OBTAINING HARDENED WORKPIECES OF FASTENERS MADE OF STAINLESS AUSTENITIC STEEL | 2020 | 
 | RU2749815C1 | 
| AUSTENITE-FERRITE HIGH-STRENGTH STEEL | 2013 | 
 | RU2522914C1 | 
| CORROSION-PROOF HIGH-STRENGTH NON-MAGNETIC STEEL AND METHOD OF THERMAL DEFORMATION PROCESSING OF SUCH STEEL | 2008 | 
 | RU2392348C2 | 
| STRENGTHENING METHOD OF FASTENERS FROM LOW-CARBON STEEL | 2013 | 
 | RU2532600C1 | 
| METHOD FOR PRODUCTION OF HIGH-STRENGTH STEEL SHEET | 2015 | 
 | RU2593810C1 | 
Authors
Dates
2010-12-10—Published
2009-11-02—Filed