FIELD: chemistry.
SUBSTANCE: invention relates to production of mineral fibre. Mineral cotton production wastes are ground to 8-50 mcm particles. Unprocessed wastes are mixed with the ground fraction in amount of 20-50%. Binder is added to the obtained mixture of components in amount of 5-10 pts. wt per 100 pts. wt, mixed and thermally treated.
EFFECT: wider base of raw materials, reduced materials consumption of the mixture and labour input during its preparation, as well as high strength of the obtained briquettes.
1 cl, 2 ex, 1 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
CHARGE FOR PRODUCTION OF MINERAL WOOL | 2003 |
|
RU2234473C1 |
ALKALI-ACTIVATED BINDER | 2022 |
|
RU2802507C1 |
METHOD OF PREPARING CHARGE FOR MINERAL FIBRE PRODUCTION | 0 |
|
SU1530577A1 |
FLOW LINE FOR MAKING MINERAL WOOL PRODUCTS | 0 |
|
SU948989A1 |
METHOD FOR PREPARING BATCH FOR MAKING MINERAL WOOL | 0 |
|
SU990689A1 |
METHOD FOR PRODUCING MINERAL WOOL | 0 |
|
SU1004278A1 |
METHOD OF PRODUCING MINERAL WOOL | 2017 |
|
RU2681172C2 |
METHOD OF MANUFACTURING HEAT-INSULATING MINERAL WOOL PRODUCTS | 2014 |
|
RU2566164C1 |
METHOD AND APPARATUS FOR CLEANING MINERAL WOOL FROM BEADS | 0 |
|
SU1006397A1 |
METHOD OF PRODUCING MINERAL WOOL | 2010 |
|
RU2439006C1 |
Authors
Dates
2010-12-27—Published
2007-12-18—Filed