FIELD: process engineering.
SUBSTANCE: invention relates to multilayer bottle intended for beer, tea, juices or carbonated drinks. Proposed bottle comprises inner and outer layers, each made from polyether (A), and, at least, one barrier layer arranged there between. Polyether (A) is thermoplastic resin produced by polymerisation of dicarboxylic acid containing 80 gram-mol or more of terephthalic acid with diol component containing 80 gram-mol or more of ethylene glycol. Barrier layer contains the mix of polyamide (B) and polyamide (C). Polyamide (B) is produced by polycondensation of diamine component containing 70% gram-mol or more of m-xylylenediamine with dicarboxylic acid containing 70 gram-mol or more of α,ω-linear aliphatic dibasic acid with C4-C20. Polyamide (C) consists of poly(6-aminocaproic acid) and/or poly(hexamethylene diamine of adipinic acid), and amorphous semi-aromatic - copolymer of hexamethylene isophthalamide/hexametgyleneamide of terephthalic acid.
EFFECT: stronger interlayer adhesion, higher resistance to lamination, good gas tightness.
12 cl, 2 tbl, 8 ex
Title | Year | Author | Number |
---|---|---|---|
MULTILAYER BOTTLE | 2006 |
|
RU2411129C2 |
MULTILAYER BOTTLE | 2006 |
|
RU2414352C2 |
METHOD OF MANUFACTURING SINGLE-LAYER PET BOTTLES WITH HIGH BARRIER AND IMPROVED TRANSPARENCY | 2004 |
|
RU2324712C2 |
NANOCOMPOSITE AND PRODUCTION METHOD THEREOF | 2008 |
|
RU2430939C2 |
METHOD OF PRODUCING MULTILAYER CONTAINER CONTAINING NANOCOMPOSITE MATERIAL | 2008 |
|
RU2412095C2 |
METHOD OF FILLING MULTILAYER BOTTLE | 2007 |
|
RU2417888C2 |
POLYAMIDE COMPOUND | 2011 |
|
RU2560880C2 |
POLYAMIDE RESIN COMPOSITION | 2007 |
|
RU2441043C2 |
POLYESTER-POLYAMIDE MIXTURES RETAINING GOOD COLOUR DURING HEAT TREATMENT | 2008 |
|
RU2475508C2 |
POLAR SOLUBLE COMPOSITIONS ABSORBING OXYGEN | 2012 |
|
RU2593453C2 |
Authors
Dates
2011-03-27—Published
2007-01-15—Filed