FIELD: metallurgy.
SUBSTANCE: coating (2) has at least one layer (3) and contains metal matrix (7) out of Ni-alloy with melting temperature lower, than material of machine element (1), with at least P as alloying component, wherein there are absorbed ceramic particles (6) of spherical shape and diameter from 40 to 160 mcm and Brinell hardness 3000. Also coating is produced by application of powder by thermal procedure.
EFFECT: reduced wear of machine parts.
18 cl, 5 dwg