FIELD: metallurgy.
SUBSTANCE: connected details of steel are assembled butt-to-butt and there is applied compression force. Butt is heated to temperature (Ac3+300)°C÷(Ac3+400)°C and conditioned at this temperature for austenisation of butt zone. Upon upset the butt is cooled with air-water mixture to temperature Mn°C÷(Mn+400)°C and is strengthened with shot. Further, the but is cooled to temperature of environment. As working substance at strengthening there are used steel balls of 0.6…0.8 diameter at air pressure 0.7…0.8 MPa.
EFFECT: raised hardness in zone of welding seam relative to base material of rail.
4 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF RAILS WELDING WITH PRESSURE AND HEATING | 2009 |
|
RU2423211C1 |
PRESSURE WELDING METHOD AT HEATING BUTT ZONE | 2006 |
|
RU2308363C1 |
PROCEDURE FOR ALUMINO-THERMAL RAIL WELDING | 2010 |
|
RU2425741C1 |
METHOD OF HEAT TREATMENT OF RAIL WELD JOINTS | 2012 |
|
RU2524526C1 |
METHOD OF THERMAL TREATMENT OF WELDED JOINTS OF RAILS | 2008 |
|
RU2371535C1 |
METHOD OF ALUMINOTHERMIC WELDING OF RAILS | 2009 |
|
RU2423212C1 |
METHOD OF ALUMINOTHERMIC WELDING OF RAILS | 2009 |
|
RU2423213C1 |
METHOD OF THERMAL TREATMENT OF WELD JOINTS OF RAILS AND DEVICE FOR IMPLEMENTATION OF METHOD | 2018 |
|
RU2705820C1 |
METHOD OF CONTACT BUTT WELDING OF RAILS | 2020 |
|
RU2743440C1 |
METHOD OF THERMAL STRENGTHENING OF RAILWAY WHEELS | 2007 |
|
RU2353672C1 |
Authors
Dates
2011-08-10—Published
2010-03-05—Filed