FIELD: textile, paper.
SUBSTANCE: method for fibrous material production consists in short-term treatment of polystyrene or its wastes in reactor with air or steam and air mixture with steam content of 50% vol. at the temperature of 90-120°C, pressure of 3 MPa for 30 seconds.
EFFECT: simple, efficient and ecologically pure method is developed for production of fibrous material from polystyrene or its wastes with high yield and good sorption properties.
9 ex, 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PRODUCING SORBENT | 2010 |
|
RU2435641C1 |
| WAY TO PRODUCE ENVIRONMENTALLY RESPONSIBLE HIGH-GRADE PETROL | 2010 |
|
RU2442767C1 |
| METHOD OF PRODUCTION OF HYDROGEN AND CARBON MATERIAL | 1999 |
|
RU2160698C1 |
| METHOD FOR PRODUCING GASOLINE FRACTIONS | 1997 |
|
RU2131905C1 |
| METHOD FOR PRODUCTION OF MOTOR FUEL COMPONENTS | 1999 |
|
RU2144056C1 |
| METHOD OF PROCESSING METHANE (VALIANTS) | 1997 |
|
RU2135441C1 |
| METHOD OF BLEACHING LINEN FIBRES FOR PRODUCTION OF MEDICAL SUPPLIES | 2013 |
|
RU2525781C1 |
| METHOD OF PRODUCING POLYSTYRENE, HAVING HIGH MELT FLOW INDEX | 2012 |
|
RU2605093C2 |
| METHOD FOR HYDROGEN FREE HYDROGENATION OF SULFATE TURPENTINE IN FLOW CONDITIONS | 2020 |
|
RU2736503C1 |
| METHOD OF SYNTHESIS OF COUPLED DIOLEFIN HYDROGENATED COPOLYMERS | 1991 |
|
RU2067589C1 |
Authors
Dates
2011-09-10—Published
2010-05-19—Filed