FIELD: construction.
SUBSTANCE: fire-resistant masonry mortar contains the following components, wt %: fire-resistant filler - used catalyst IM-2201 with the following content, wt %: Al2O3 - 72.5 and Cr2O3 - 16.2, 70-80; fire-resistant clay - mechanically and chemically activated, 15-25; sodium tripolyphosphate 0.5-1.0; water - balance.
EFFECT: increased strength after sintering.
1 ex, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
MIX FOR PRODUCTION OF CASTING RODS HARDENED IN HEATED TOOLING, METHOD OF ITS PRODUCTION | 2010 |
|
RU2440211C2 |
FIRE-RESISTANT MASONRY ADMIXTURE | 2011 |
|
RU2460705C1 |
REFRACTORY MASONRY MORTAR | 1995 |
|
RU2101256C1 |
REFRACTORY LAYING MATERIAL | 1995 |
|
RU2100319C1 |
EXOTHERMIC REFRACTORY MORTAR | 1996 |
|
RU2163579C2 |
PARTING PAINT FOR MOLDS AND RODS | 2019 |
|
RU2722845C1 |
CATALYST, METHOD FOR PRODUCTION THEREOF AND PROCESS FOR DEHYDROGENATION OF C-C PARAFFIN HYDROCARBONS INTO OLEFIN HYDROCARBONS USING SAID CATALYST | 2014 |
|
RU2546646C1 |
NON-STICK COATING FOR MOLDS AND RODS | 2018 |
|
RU2689473C1 |
REFRACTORY COMPOSITION | 1994 |
|
RU2081089C1 |
REFRACTORY LIQUID | 1991 |
|
RU2062764C1 |
Authors
Dates
2011-09-27—Published
2009-12-22—Filed