FIELD: construction.
SUBSTANCE: fused refractory material has the following composition, wt %: 0.3-0.7 Na2O; 1.0-1.5 CaO; 1.0-2.0 Cr2O3; 0.5-1.0 MgO; 0.2-0.8 SiO2; Al2O3 - balance. Fused material has good compressibility and sintering ability, has high temperature of load softening start.
EFFECT: improved physical-chemical and thermomechanical properties, increased density of material.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
FUSED REFRACTORY MATERIAL | 2014 |
|
RU2574236C2 |
MAGNESIA SPINEL-BASED FUSED MATERIAL AND METHOD OF PRODUCING SAID MATERIAL | 2009 |
|
RU2417201C2 |
MOLTEN REFRACTORY MATERIAL | 2008 |
|
RU2371422C1 |
FUSED FORSTERITE-CONTAINING MATERIAL AND METHOD OF OBTAINMENT | 2008 |
|
RU2367632C1 |
CHROMOUS CALCIUM HEXAALUMINATE-BASED REFRACTORY AGGREGATE AND PRODUCTION METHOD THEREOF | 2009 |
|
RU2401820C1 |
MELT-MOULDED CHROMIUM-CONTAINING REFRACTORY MATERIAL | 2012 |
|
RU2495000C2 |
MELT-MOULDED HIGH-CHROMIUM REFRACTORY MATERIAL | 2015 |
|
RU2581182C1 |
ELECTROCORUNDUM AND METHOD OF MAKING IT | 2007 |
|
RU2347766C2 |
CHARGE FOR MANUFACTURE OF ALUMINIUM-FERROUS SPINEL AND REFRACTORY USING ALUMINIUM-FERROUS SPINEL | 2013 |
|
RU2541997C1 |
MELTED CHROME-CONTAINING REFRACTORY MATERIAL | 1992 |
|
RU2041181C1 |
Authors
Dates
2011-10-20—Published
2010-04-26—Filed