FIELD: chemistry.
SUBSTANCE: mixture for producing coloured glass contains the following in wt %: soda 3.0-4.0; quartz sand 34.5-35.75; borax 50.0-55.0; bone ash 5.0-10.0; cobalt sulphate 0.25-2.5. The melting temperature is equal to 1100-1250°C.
EFFECT: low melting temperature of the glass.