FIELD: construction.
SUBSTANCE: high-strength concrete contains portland cement, sand, crushed stone, water and an additive that includes calcium chloride, sols of silicic acid and iron and aluminium hydrogen oxides. The additive has density of 1.041 g/cm3, pH=1.4 with subsequent ratio of components, wt %: portland cement 19.3-23.3; sand 29.2-30.4; crushed stone 38.10-40.10; specified additive 0.07-0.1; water 9.3-10.1.
EFFECT: increased compression strength at rated age with lower additive consumption.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
HIGH-STRENGTH CONCRETE | 2007 |
|
RU2331602C1 |
HIGH STRENGTH CONCRETE | 2023 |
|
RU2801191C1 |
HIGH-STRENGTH CONCRETE | 2019 |
|
RU2717021C1 |
HIGHT-STRENTH CONCRETE | 2006 |
|
RU2332388C1 |
HIGH-STRENGTH CONCRETE | 2016 |
|
RU2610488C1 |
HIGH-STRENGTH CONCRETE | 2006 |
|
RU2332379C1 |
HIGH-STRENGTH CONCRETE | 2016 |
|
RU2614177C1 |
HIGH STRENGTH CONCRETE | 2022 |
|
RU2781587C1 |
HIGH-STRENGTH CONCRETE | 2016 |
|
RU2616964C1 |
HIGH-STRENGTH CONCRETE | 2015 |
|
RU2593402C1 |
Authors
Dates
2012-01-20—Published
2010-06-16—Filed