FIELD: metallurgy.
SUBSTANCE: concentrate is subjected to two-stage oxidising roasting. Note here that, before first stage, said concentrate is mixed with sulfur-binding additive to perform first roasting stage at 550-650°C for 15-30 min. Prior to second roasting stage, molybdenum concentrate is added to calcine produced at first stage in amount of 10-30 wt % from concentrate used in first roasting step. Second roasting is performed at 600-670°C for 30-40 min with subsequent leaching of molybdenum and rhenium from calcine obtained in first step.
EFFECT: higher yield of molybdenum.
2 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PROCESSING MOLYBDENITE-CONTAINING CONCENTRATES | 2018 |
|
RU2696989C1 |
METHOD OF PROCESSING SULPHIDE AND MIXED MOLYBDENUM-CONTAINING CONCENTRATES FOR EXTRACTION OF MOLYBDENUM AND RHENIUM | 2009 |
|
RU2393253C1 |
METHOD OF PROCESSING MOLYBDENITE CONCENTRATES AND MIDDLINGS | 2001 |
|
RU2191840C1 |
PROCESSING METHOD OF MOLYBDENITE CONCENTRATES | 2014 |
|
RU2550981C1 |
PROCESSING METHOD OF MOLYBDENITE CONCENTRATES | 2012 |
|
RU2493280C1 |
METHOD FOR PROCESSING OF SULPHIDE AND MIXED MOLYBDENUM-CONTAINING CONCENTRATES | 2013 |
|
RU2536615C1 |
METHOD OF PROCESSING SULPHIDE AND MIXED MOLYBDENUM-CONTAINING CONCENTRATES | 2019 |
|
RU2703757C1 |
PROCESSING METHOD OF MOLYBDENITE CONCENTRATES | 2014 |
|
RU2548341C1 |
METHOD OF PROCESSING OF MOLYBDENUM INTERMEDIATE PRODUCT | 2000 |
|
RU2158778C1 |
METHOD OF HYDROMETALLURGICAL PROCESSING OF RHENIUM-CONTAINING MOLYBDENUM RAW MATERIAL | 2019 |
|
RU2693223C1 |
Authors
Dates
2012-01-27—Published
2010-03-04—Filed