FIELD: metallurgy.
SUBSTANCE: method for processing of sulphide and mixed molybdenum-containing concentrates involves mixing of concentrates with an additive of calcium oxide taken in the quantity of 2-2.5 times excess of the stoichiometrically required one for connection of molybdenum, rhenium and sulphur at oxidation annealing into non-volatile compounds. Then, oxidation annealing of the mixture is performed during 60-120 minutes. Leaching of the obtained stub end is performed in two stages. Water leaching is performed at the first stage during 60-80 minutes at S:L ratio of at least 1:2 and temperature of 90-95°C for selective extraction of rhenium into the solution. At the second stage, leaching is performed by means of a solution of alkali metal carbonate for extraction into the solution of molybdenum and the rest rhenium.
EFFECT: improving efficiency of the method and selective separation of molybdenum and rhenium.
2 cl, 1 dwg, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING SULPHIDE AND MIXED MOLYBDENUM-CONTAINING CONCENTRATES | 2019 |
|
RU2703757C1 |
METHOD OF PROCESSING SULPHIDE AND MIXED MOLYBDENUM-CONTAINING CONCENTRATES FOR EXTRACTION OF MOLYBDENUM AND RHENIUM | 2009 |
|
RU2393253C1 |
METHOD FOR PROCESSING MOLYBDENITE-CONTAINING CONCENTRATES | 2018 |
|
RU2696989C1 |
METHOD OF MOLYBDENUM CONCENTRATE PROCESSING | 2010 |
|
RU2441084C2 |
METHOD FOR COMPLEX PROCESSING OF SULPHIDE-OXIDISED COPPER-PORPHYRITIC ORES | 2018 |
|
RU2685621C1 |
METHOD OF HYDROMETALLURGICAL PROCESSING OF RHENIUM-CONTAINING MOLYBDENUM RAW MATERIAL | 2019 |
|
RU2693223C1 |
METHOD FOR PROCESSING SPENT MOLYBDENUM-ALUMINIUM-CONTAINING CATALYST | 2017 |
|
RU2645825C1 |
METHOD OF PROCESSING MOLYBDENITE CONCENTRATES AND MIDDLINGS | 2001 |
|
RU2191840C1 |
PROCESSING METHOD OF WASTE MOLYBDENUM-ALUMINIUM-CONTAINING CATALYST | 2011 |
|
RU2466199C1 |
METHOD OF MOLYBDENUM CALCINE PROCESSING | 0 |
|
SU1801139A3 |
Authors
Dates
2014-12-27—Published