FIELD: metallurgy.
SUBSTANCE: method for improving qualitative indices of blast-furnace coke is implemented by spraying at temperature of not less than 20°C onto blast-furnace coke lumps of 2-20% water solution of sodium, potassium or calcium pentaborate, which contains 0.1-0.2 wt % of non-ionic surface active substance in the form of mono- and/or dialkyl ethers of polyethylene glycol in the quantity providing the content of surface active substance in coke of 0.0035-0.0070 wt %; at that, content of dry pentaborate of one of the above metals in coke is 0.09-0.68 wt %.
EFFECT: improving qualitative indices of blast-furnace coke owing to decreasing reactivity index and increasing its strength value.
1 cl, 25 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING HIGH-QUALITY COKE | 2013 |
|
RU2539186C1 |
FURNACE COKE PROCESSING METHOD | 2007 |
|
RU2336297C1 |
METHOD OF PREPARATION OF COAL, INCLUDING HIGH-SULPHUR, FOR COKING | 2013 |
|
RU2530109C2 |
METHOD OF PRODUCING MINERAL WOOL | 2010 |
|
RU2439006C1 |
METHOD OF PRODUCING NICKEL MATTE | 2010 |
|
RU2441082C1 |
METHOD OF DETERMINATION OF FULL MELT OUTLET DURING BLAST-FURNACE SMELTING | 2014 |
|
RU2558840C1 |
METHOD OF PRODUCING COPPER MATTE | 2010 |
|
RU2441080C1 |
METHOD OF PYROMETALLURGICAL PROCESSING OF COPPER-CONTAINING MATERIALS | 2010 |
|
RU2441081C1 |
METHOD FOR CHANGING THE PROPERTIES OF COAL CONCENTRATES | 2021 |
|
RU2782029C1 |
METHOD OF BLAST-FURNACE MELTING | 2008 |
|
RU2359041C1 |
Authors
Dates
2012-03-20—Published
2011-03-21—Filed