FIELD: metallurgy.
SUBSTANCE: method involves treatment of parts with pulse current in electrolyte containing the following, g/l: boric acid 8-12, ethanedioic acid 15-20, borax 10-12, magnesium sulphate 15-20 and ammonium paratungstate 5-7. Treatment is performed at electrolyte temperature of 18-22°C. Amplitude of current pulse of cathode half-period is 0.15-0.25 of current pulse amplitude of anode half-period. Treatment is performed at current density of 1.2-1.6 A/cm2.
EFFECT: method allows improving the structure of oxide film, obtaining high regularity degree of porous structure, improving film elasticity and enlarging diameter of pores.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF THICK-LAYERED ANODIZING OF FLAT ALUMINIUM PRODUCTS | 1994 |
|
RU2062824C1 |
METHOD OF PRODUCING ALUMINIUM OXIDE-BASED PHOTOCONVERTER | 2013 |
|
RU2548402C1 |
METHOD OF MAKING ALUMINIUM OXIDE-BASED MEMBRANES | 2011 |
|
RU2474466C1 |
METHOD FOR BUILDING-UP BARRIER COATING ON SOLDERED ALUMINIUM ELECTRODES OF OZONE GENERATOR | 2016 |
|
RU2640586C1 |
METHOD OF ELECTROCHEMICAL COLOURING OF ANODISED ALUMINIUM BY VARIABLE-POLARITY CURRENT (VERSIONS) | 2011 |
|
RU2467096C2 |
PROCESS TO MANUFACTURE POROUS ANODIC ALUMINA | 2006 |
|
RU2324015C1 |
METHOD OF PROTECTING INSULATION COATING ON ZIRCONIUM | 2011 |
|
RU2472873C1 |
METHOD OF APPLYING ELECTROCONDUCTIVE PROTECTIVE COATING ON ALUMINIUM ALLOYS | 2023 |
|
RU2817277C1 |
TECHNIQUE OF OXIDE COATING ON ALUMINIUM AND ITS ALLOYS | 2007 |
|
RU2353717C1 |
ELASTIC ALUMINA NANO-MEMBRANE OBTAINING METHOD | 2017 |
|
RU2678055C2 |
Authors
Dates
2012-04-20—Published
2010-12-30—Filed