FIELD: machine building.
SUBSTANCE: using mould recovery method in the manufacture of production tooling, made of silicon elastic material, the surface of a mould is pre-treated with a solution of amine or amine mixture in an organic solvent. Then repair mortar is applied, containing high molecular weight silicone rubber, a curing agent and an organic solvent, which additionally may contain a solution of amine or amine mixture in an organic solvent. The invention also relates to a composition for restoring of moulds, made of silicone elastic material. The composition contains a high molecular weight silicone rubber, a curing agent, an organic solvent solution of an amine or a mixture of amines in an organic solvent at a ratio of the wt % - Amine: rubber from 1:20 to 1:50.
EFFECT: when restoring a damaged mould the surface is hardened that prolongs the use of a mould, ensures good traction with the surface of the mould, curing of reducing layer is accelerated, its uniformity is achieved on a complex profile of a mould.
3 cl, 2 dwg, 2 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR THE ELASTIC COATING OF THE MOLDS AT MANUFACTURE OF THE PRODUCTION TOOLS | 2004 |
|
RU2277553C2 |
METHOD OF PRODUCING SILICONE ADHESIVE AND ADHESIVE COMPOSITION | 2009 |
|
RU2467048C2 |
ORGANOSILICON ELASTIC MOULDING COMPOUND | 2010 |
|
RU2443733C1 |
POLYMER COMPOSITION FOR ABSORBING HIGH-FREQUENCY ENERGY | 2012 |
|
RU2493186C1 |
POLYMER COMPOSITE MATERIAL FOR RADIOELECTRONIC EQUIPMENT | 2012 |
|
RU2502767C2 |
FORMATION METHOD OF PROTECTIVE COATING, AND COMPOSITION FOR COATING | 2011 |
|
RU2454842C1 |
STRENGTHENED ANTIADHESIVE ORGANOSILICON COMPOSITION | 1992 |
|
RU2081142C1 |
REPAIR ADHESIVE COMPOSITION | 2009 |
|
RU2412973C1 |
COMPOSITION OF COATING OF STRIP PAPER FOR MEDICAL ADHESIVE FILMS | 0 |
|
SU1395721A1 |
METHOD OF COLD HARDENING SILICON-ORGANIC ANTIADHESIVE COATING PRODUCTION | 1992 |
|
RU2080995C1 |
Authors
Dates
2012-07-20—Published
2010-10-06—Filed