FIELD: chemistry.
SUBSTANCE: base of the polymer electrolyte gel used is a dispersion of a vinyl acetate and acrylate copolymer in organic solvents, with the following ratio of components of the mixture (wt % of dry substance): anhydrous ionic inorganic lithium salt 15-30, anhydrous organic solvent 30-40, vinyl acetate/acrylate copolymer 30-55, wherein the obtained electrolyte has moisture content less than 0.003%.
EFFECT: high adhesion capacity, elasticity, low environmental risk and low production cost.
5 ex
Title | Year | Author | Number |
---|---|---|---|
PREPARATION METHOD OF GEL ELECTROLYTE FOR LITHIUM-ION CELLS | 2009 |
|
RU2414777C1 |
METHOD FOR MANUFACTURING OF LITHIUM-ION ACCUMULATOR ELECTRODES | 2014 |
|
RU2547819C1 |
LITHIUM-POLYMER BATTERY AND METHOD OF ITS MANUFACTURING | 2014 |
|
RU2564201C1 |
POLYMER GEL ELECTROLYTE FOR LITHIUM-ION BATTERIES | 2023 |
|
RU2814465C1 |
GEL POLYMER ELECTROLYTE AND CURRENT SOURCE USING IT | 2009 |
|
RU2424252C2 |
ADDITIVES FOR GALVANIC CELLS | 2013 |
|
RU2665552C2 |
METHOD FOR MANUFACTURING RECHARGEABLE LITHIUM-POLYMER BATTERIES AND BATTERY MANUFACTURED BY THIS METHOD | 2001 |
|
RU2262779C2 |
METHOD FOR MANUFACTURING OF LITHIUM-ION ACCUMULATOR ELECTRODES | 2008 |
|
RU2390078C1 |
METHOD FOR MANUFACTURING OF LITHIUM-ION ACCUMULATOR | 2009 |
|
RU2404489C1 |
LITHIUM-ION BATTERY WITH OPERATING RANGE EXPANDED INTO LOW TEMPERATURE RANGE | 2017 |
|
RU2728531C2 |
Authors
Dates
2012-07-27—Published
2011-01-11—Filed