FIELD: chemistry.
SUBSTANCE: article has a bearing rod and a reinforcing winding made from fibre filler saturated with polymer binder. The polymer binder contains the following (wt %): epoxy resin 8-14, isomethyl tetrahydrophthalic anhydride 8-14, polymerisation accelerator 0.4-1.0 and a modifying additive - aromatic conjugated hydroxyphenylene 1.8-3.0. The fibre filler is made from mineral carbon fibre.
EFFECT: invention improves operational characteristics of the composite reinforcing article.
3 cl, 1 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
POLYMER BINDER FOR COMPOSITE REINFORCEMENT | 2010 |
|
RU2495892C2 |
COMPOSITE REINFORCEMENTS | 2012 |
|
RU2509653C1 |
MODIFIED POLYMER COMPOSITE REINFORCEMENT | 2023 |
|
RU2826026C1 |
CONCRETE-REINFORCING ROD | 2001 |
|
RU2220049C2 |
METHOD OF MAKING ARTICLES FROM COMPOSITE | 2012 |
|
RU2505403C1 |
ENAMEL FOR PROTECTIVE COATING | 2011 |
|
RU2472829C1 |
ROD FOR CONCRETE REINFORCEMENT AND METHOD OF ITS MANUFACTURING | 2008 |
|
RU2381905C2 |
METHOD FOR PRODUCING HIGH-STRENGTH COMPOSITE REINFORCEMENT | 2022 |
|
RU2799001C1 |
COMPOSITION TO REINFORCE BUILDING STRUCTURES | 2012 |
|
RU2493337C1 |
METHOD OF PRODUCING POLYMERIC COMPOSITE MATERIALS | 2016 |
|
RU2637227C1 |
Authors
Dates
2012-09-20—Published
2011-04-01—Filed