FIELD: chemistry.
SUBSTANCE: bitumen-polymer composition is prepared from polymer crumbs - butadiene styrene thermoplastic elastomer DST-30 and wastes from production of synthetic rubber and latex with Defo hardness of 2700, butimen, mineral filler - chalk, resin 101 K and industrial oil wastes. First, the polymers are crushed to particle size deq≤0.018 m and molten BNK 90/30 bitumen is prepared. The crushed polymers, molten, chalk, resin 101 K and industrial oil wastes are fed to rollers which are preheated to temperature 50-80°C. The mixing process is carried out until achieving complete homogenisation. The specific time of mixing is 3.5-5.5 minutes. The composition is prepared with the following ratio of components in wt %: bitumen BNK 90/30 41.0, butadiene styrene thermoplastic elastomer DST-30 - 24.0, and wastes from production of synthetic rubber and latex with Defo hardness of 2700 - 23.0, mineral filler - chalk - 9.0, resin 101 K - 1.0, industrial oil wastes -2.0.
EFFECT: reduced time energy and time spent on producing the composition; the obtained composition has improved physical and mechanical properties.
1 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF BITUMEN-POLYMERIC COMPOSITIONS | 2002 |
|
RU2218370C1 |
WATER-PROOFING AND ADHESIVE SEALING COMPOSITION | 2011 |
|
RU2478113C2 |
POLYMERIC COMPOSITION | 2006 |
|
RU2320682C1 |
WATER-PROOFING AND SEALING ADHESIVE COMPOSITION | 2006 |
|
RU2406743C2 |
HYDROINSULATING AND SEALING-ADHESIVE COMPOSITION | 1999 |
|
RU2165949C2 |
BITUMEN COMPOSITION, AND A METHOD OF ITS PREPARING | 1991 |
|
RU2011667C1 |
SEALING AND ADHESIVE COMPOSITION AND METHOD OR PREPARING THEREOF | 1998 |
|
RU2142490C1 |
METHOD OF CONTROLLING QUALITY PARAMETERS OF BITUMEN-POLYMER COMPOSITION | 2014 |
|
RU2568916C1 |
METHOD OF PROCESSING POLYMER WASTES | 2010 |
|
RU2465132C2 |
BITUMEN-POLYMER BINDER | 2000 |
|
RU2184751C2 |
Authors
Dates
2012-09-20—Published
2011-04-19—Filed