FIELD: chemistry.
SUBSTANCE: composition has the following component ratio, wt %: non-specified synthetic rubber SKD - structured production wastes - 17.0-20.0; non-specified synthetic rubber SKS - production wastes - 23.0-25.0; bitumen BNK-90/30 - 18.0-20.5; alkylphenol resin-octophore-N - 2.0-1.5; chalk -20.0-12.0; kaolin - 5.0-3.0; industrial oil wastes -15.0-18.0.
EFFECT: high quality of the water-proofing and adhesive sealing composition owing to improved physical and mechanical properties thereof and low water absorption thereof.
1 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING BITUMEN-POLYMER COMPOSITIONS | 2011 |
|
RU2461593C1 |
WATER-PROOFING AND SEALING ADHESIVE COMPOSITION | 2006 |
|
RU2406743C2 |
HYDROINSULATING AND SEALING-ADHESIVE COMPOSITION | 1999 |
|
RU2165949C2 |
POLYMERIC COMPOSITION | 2006 |
|
RU2320682C1 |
METHOD OF CONTROLLING QUALITY PARAMETERS OF BITUMEN-POLYMER COMPOSITION | 2014 |
|
RU2568916C1 |
SEALING AND ADHESIVE COMPOSITION AND METHOD OR PREPARING THEREOF | 1998 |
|
RU2142490C1 |
ROOFING MATERIAL | 2004 |
|
RU2278876C1 |
BITUMEN-POLYMER BINDER | 2000 |
|
RU2184751C2 |
METHOD OF PRODUCTION OF BITUMEN-POLYMERIC COMPOSITIONS | 2002 |
|
RU2218370C1 |
COMPOSITION FOR COATING FLOORS | 0 |
|
SU1054095A1 |
Authors
Dates
2013-03-27—Published
2011-05-13—Filed