FIELD: chemistry.
SUBSTANCE: composition contains 50-70 wt % heterophase propylene copolymer, 2-10 wt % ethylene and alpha-olefin based elastomer, 20-46 wt % inorganic filler and at least two different α-crystal-nucleating agents, total weight content of which ranges from 0.0011 to 2.0%. The heterophase propylene copolymer contains 70-90 wt % propylene homopolymer with respect to the weight of the heterophase propylene copolymer and 10-30 wt % ethylene-propylene rubber with respect to the weight of the heterophase propylene copolymer, and the alpha-olefin used in the ethylene and alpha-olefin based elastomer is C4-C10 alpha-olefin.
EFFECT: defined ratio of components of the composition ensures balance of its properties, combination of low coefficient of linear thermal expansion, high rigidness and high temperature of thermal deformation.
11 cl, 2 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
AUTOMOBILE MATERIAL WITH EXCELLENT FLUID FLOW CHARACTERISTICS, HIGH RIGIDITY, EXCELLENT PLASTICITY AND LOW COEFFICIENT OF LINEAR THERMAL EXPANSION (CLTE) | 2010 |
|
RU2520448C2 |
METHOD FOR OBTAINING HETEROPHASIC POLYMER COMPOSITIONS | 2020 |
|
RU2799757C2 |
CROSS-LINKABLE POLYOLEFIN COMPOSITION | 2018 |
|
RU2730523C1 |
PROPYLENE POLYMERS | 2007 |
|
RU2441028C2 |
VISCOUS PROPYLENE COMPOSITION WITH GOOD DIMENSIONAL STABILITY AND EXCELLENT SURFACE APPEARANCE | 2017 |
|
RU2699810C1 |
ARTICLE FOR CAR INTERIOR DECORATION HAVING REDUCED ODOUR | 2010 |
|
RU2506288C2 |
HETEROPHASE POLYPROPYLENE COPOLYMER COMPOSITION | 2010 |
|
RU2510407C2 |
THERMOPLASTIC POLYOLEFINS WITH HIGH FLUIDITY AND EXCELLENT SURFACE QUALITY, OBTAINED IN MULTISTEP PROCESS | 2009 |
|
RU2470963C2 |
COMPOSITION MATERIAL WITH FILLER ON BASIS OF CELLULOSE | 2016 |
|
RU2679149C1 |
POLYPROPYLENE COMPOSITION | 2019 |
|
RU2758954C1 |
Authors
Dates
2012-10-20—Published
2009-07-10—Filed