FIELD: metallurgy.
SUBSTANCE: pellet manufacturing charge includes manganese raw material in the form of manganese concentrate, slag formation flux, reducing agent and binding agent. As binding agent, it contains slag as a result of melting of metal manganese, which is pre-crushed till specific surface area of 450-500 m2/kg in quantity of 7-14%. Water is added to the above charge, pellets are made and subject to hydration, and hardening and drying is performed at room temperature.
EFFECT: increasing mechanical strength of pellets, reducing the amount of moisture in pellets, decreasing the sintering temperature and reducing the consumption of carbonaceous materials.
2 cl, 2 tbl, 1 ex
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD FOR REMOVING PHOSPHORUS FROM MANGANESE RAW MATERIAL | 2011 |
|
RU2465351C1 |
| BINDER AND METHOD OF ITS MAKING | 2009 |
|
RU2416580C1 |
| BINDER | 2008 |
|
RU2366627C1 |
| CLINKERLESS CEMENT | 2010 |
|
RU2430043C1 |
| PURIFICATION METHOD OF FERROMANGANESE RAW MATERIALS FROM PHOSPHOROUS | 2008 |
|
RU2360987C1 |
| PROCEDURE FOR PURIFICATION OF MANGANESE CONCENTRATES FROM PHOSPHORUS | 2009 |
|
RU2395601C1 |
| BUILDING MIXTURE AND METHOD OF CONCRETE PRODUCTION | 2008 |
|
RU2377213C1 |
| PROCEDURE FOR MANGANESE ORE COMPLEX PROCESSING | 2010 |
|
RU2432405C1 |
| CINDER BINDER | 2010 |
|
RU2448063C2 |
| RAW MIX FOR PREPARATION OF FROST-RESISTANT WALL BUILDING STONES AND MONOLITHIC WALLS | 2011 |
|
RU2484067C2 |
Authors
Dates
2012-10-20—Published
2010-08-20—Filed