FIELD: construction.
SUBSTANCE: cement produced by grinding of a mixture containing the following components, wt %: blast furnace slag - 40-50; calcium sulfate dihydrate - 4-6; wastes of iron ores enrichment 3-6; sodium or potassium, or ammonium carbonates or their mixture - 3-8; steel smelting slag - electric steel smelting, open-hearth or converter one - balance. Besides, the mixture is ground down to specific surface of 700 m2/kg.
EFFECT: increased strength and frost resistance of cement.
1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
BINDING AGENT | 2000 |
|
RU2186043C2 |
BINDER | 2008 |
|
RU2363673C1 |
BINDER AND METHOD OF ITS MAKING | 2009 |
|
RU2416580C1 |
CINDER BINDER | 2010 |
|
RU2448063C2 |
BINDER | 2008 |
|
RU2376251C1 |
RAW MIX AND METHOD FOR PRODUCTION OF CONCRETE FROM IT | 2008 |
|
RU2378214C1 |
BINDER | 2008 |
|
RU2366627C1 |
BINDER AND METHOD OF ITS PREPARATION FOR PRODUCTION OF DECORATIVE CONCRETE | 2010 |
|
RU2452702C1 |
BINDER | 2008 |
|
RU2368577C1 |
BINDER | 2008 |
|
RU2363674C1 |
Authors
Dates
2011-09-27—Published
2010-08-20—Filed