FIELD: construction.
SUBSTANCE: glaze charge contains the following components, wt %: quartz sand 62.5-66.2; lead minium 12-16; potash 4-6; soda 4-6; cobalt oxide 0.3-0.5; copper oxide 1-1.5; cryolite 4-6; stannum dioxide 4-6.
EFFECT: increase of glaze frost resistance.
1 tbl