FIELD: machine building.
SUBSTANCE: described composition contains the following: Tremolite Ca2Mg5Si8O22(OH)2 - 50-53%; Lizardite Mg3Si2O5(OH)4 - 31-35%; Antigorite Mg6{Si4O10}(OH)8 - 9-12%; Magnetite FeO-FeO3 - 3-7%. Magnetite has average particle size of 1.5 mcm. The above composition can be used as an additive to lubricants, as solid lubricant or running-in composition used during repair of friction assemblies with disassembly of assemblies of machines and mechanisms.
EFFECT: improvement of anti-friction and wear-resistant properties of friction assemblies, including friction assemblies with increased microhardness.
| Title | Year | Author | Number | 
|---|---|---|---|
| COMPOSITION "FRICTION GEOMODIFIER" FOR UNDEMOUNTABLE IMPROVEMENT OF TRIBOTECHNICAL CHARACTERISTICS OF FRICTION UNITS | 1999 | 
 | RU2169172C1 | 
| COMPOSITION FOR IMPROVING OF FRICTION ASSEMBLY ENDURANCE | 2002 | 
 | RU2246531C2 | 
| ANTIWEAR, ANTIFRICTION RESTORATION TRIBOTECHNICAL COMPOSITION | 2015 | 
 | RU2599161C1 | 
| NANOTECHNOLOGY-BASED ANTIFRICTION POWDERED COMPOSITION (VERSIONS), NANOTECHNOLOGY-BASED LUBRICANT COMPOSITION AND NANOTECHNOLOGY-BASED LUBRICATION METHOD | 2009 | 
 | RU2415176C2 | 
| BREAK-IN OIL FOR INTERNAL COMBUSTION ENGINES | 2005 | 
 | RU2313565C2 | 
| COMPOUND FOR FORMING LAYER ON FRICTION METAL SURFACES | 2004 | 
 | RU2266979C1 | 
| FRICTION MODIFIER | 2009 | 
 | RU2420562C1 | 
| PROCEDURE FOR APPLICATION OF ANTI-FRICTION COATING ON CONTACT RUBBING SURFACES OUT OF ULTRA-DISPERSED COMPOSITION AND FORMULATION OF ULTRA-DISPERSED COMPOSITION | 2009 | 
 | RU2421547C1 | 
| METHOD OF PRODUCING RECOVERABLE ANTIFRICTION AND WEAR-RESISTANT COAT FOR MACHINERY ASSEMBLY UNITS AND PARTS | 2008 | 
 | RU2345176C1 | 
| METHOD OF MODIFICATION OF IRON-CONTAINING SURFACES OF FRICTION UNITS | 2001 | 
 | RU2201998C2 | 
Authors
Dates
2012-12-10—Published
2011-08-16—Filed